Abstract

This paper presents the realization of TiC thin films by CVD method. The thin layers of TiC thicknesses were 8 and 10 μm, their thickness increasing with time, keeping the temperature. Diffractometer analysis certifies that this thin layer of TiC is homogeneous and unscratched. Microhardness of thin layers of TiC is HV0,05 = 30000 MPa compared to WC (carbide substrate of the component) that has a microhardness HV0,05 = 17000MPa.

Creative Commons License

Downloads

Download data is not yet available.

Downloads

Published

2013-09-15

Issue

Section

Articles

How to Cite

1.
Characterization of Sintered Hardmetals Coated with TiC. Ann_UGAL_MMS [Internet]. 2013 Sep. 15 [cited 2026 Nov. 2];36(3):50-4. Available from: https://ojs.ugal.ro/index.php/mms/article/view/2744

Most read articles by the same author(s)

1 2 3 > >>