On the Optimization of Machined VSD Position for Repaired Pipes
DOI:
https://doi.org/10.35219/mms.2025.2.04Keywords:
pipes, volumetric defects, optimizationAbstract
To be kept in use, pipelines with Volumetric Surface Defects (VSDs) must be evaluated and, if necessary, repaired. The first step in the repair process is machining the defect area. In all cases, the machined defect has a rectangular shape, with edges parallel/perpendicular to the pipe axis. We propose a novel approach: the VSD is scanned, the image is then processed using segmentation techniques, the VSD contour is detected, and finally, a family of rectangles with minimal area enclosing the VSD is defined. After that, a Finite Element Analysis is performed for each machined VSD, and an optimal case is selected.
Downloads
Download data is not yet available.
Downloads
Published
2025-06-15
Issue
Section
Articles
How to Cite
1.
On the Optimization of Machined VSD Position for Repaired Pipes. Ann_UGAL_MMS [Internet]. 2025 Jun. 15 [cited 2026 Nov. 2];48(2):25-31. Available from: https://ojs.ugal.ro/index.php/mms/article/view/9236